Location:Home > Building Materials
  • Jade spar process

     

    ◎ the silica sand, feldspar, calcium carbonate, harmonic mixing special materials.
    ◎ molten material in the melting furnace (about 1600 ℃ or so).
    ◎ molten glass paste with water to form 1-7mm quenched glass particle size.
    ◎ particles into the glass and then kiln dried
    ◎ flat on the fire resistance of glass particles on the template, into the roller kiln firing, the glass heated to 850 ℃, the beginning of grain began to melt, 950 ℃ began to melt the glass particles and precipitation of needle-like crystals, 1100 ℃ crystallization completed.
    ◎ The initial crystallization plate to complete cooling
    ◎ jade spar at the back of paste FRP (glass fiber mesh) to prevent the completion of construction of the wall plate subjected to physical shock will break falling
    ◎ jade spar to be several times appeared on the surface grinding
    ◎ luster and texture of crystal clear cut into 900 mm X 900 mm, 900 mm X 1200 mm plate size, upright storage
     ◎ board account in steel shelves and cover with plastic corner protection and plastic sheets covering the designed camber size
     ◎ need to bend from the heating